| 中國醫藥大學 |
1998-04 |
The influence of electrical stimulation on strength of quadriceps femoris in healthy male.
|
(Sun S.-H); (Wu S.-K); 郭美英(Mei-Ying kuo); (Lin C.-Y); (Chang Y.-H) |
| 國立臺灣大學 |
1998 |
A Study on Lattice Parameters of Martensite in Ti50.5-xNi49.5Zrx Shape Memory Alloys
|
Hsieh, S.F.; Wu, S.K. |
| 國立臺灣大學 |
1998 |
Infrared Joining of TiAl Intermetallics Using Ti-15Cu-15Ni Foil, Part I: The Microstructure Morphologies of Joint Interfaces
|
Lee, S.J.; Wu, S.K.; Lin, R.Y. |
| 國立臺灣大學 |
1998 |
Room Temperature Phases Observed in Ti53-xNi47Zrx High Temperature Shape Memory Alloys
|
Hsieh, S.F.; Wu, S.K. |
| 國立臺灣大學 |
1998 |
The Deformation Texture in a Ti49Ni51 Alloy
|
Chou, T.S.; Wu, S.K.; Lin, H.C. |
| 國立臺灣大學 |
1998 |
Infrared Joining of TiAl Intermetallics Using Ti-15Cu-15Ni Foil, Part II: The Microstructure Evolution at High Temperature
|
Lee, S.J.; Wu, S.K.; Lin, R.Y. |
| 國立臺灣大學 |
1998 |
A Study on Ternary Ti-rich TiNiZr Shape Memory Alloys
|
Hsieh, S.F.; Wu, S.K. |
| 國立臺灣大學 |
1998 |
A Study of the Deformation Texture on A Ti49Ni51 Alloy
|
T.S.Chou; 吳錫侃; Lin, H.C.; T.S.Chou; Wu, S.K.; Lin, H.C. |
| 國立臺灣大學 |
1997 |
Ion nitriding of equiatomic TiNi shape memory alloys II. Corrosion properties and wear characteristics
|
Wu, S.K.; Lin, H.C.; Chu, C.L. |
| 國立臺灣大學 |
1997 |
The Microstructural Evolution of Infrared Joining of TiAl Intermerallics Using Ti-15Cu-15Ni Foil
|
Lee, S.J.; Wu, S.K.; Wang, J.Y. |
| 國立臺灣大學 |
1997 |
Oxidation improvement of Ti-48Al-2Cr-2Nb intermetallics by air plasma sprayed ZrO2-Ni-4.5wt.%Al coatings
|
Hsu, I.C.; Wu, S.K. |
| 國立臺灣大學 |
1997 |
Ion nitriding of TiNi shape memory alloys I. Nitriding parameters and microstructure characterization
|
Wu, S.K.; Lin, H.C.; Chu, C.L. |
| 國立臺灣大學 |
1997 |
A study of vacuum carburization of an equiatomic TiNi shape memory alloy
|
Lee, G.Y.; Wu, S.K.; Lin, H.C. |
| 國立臺灣大學 |
1997 |
A study of aluminum cladding on Ti50Al50 intermetallics by liquid aluminizing
|
Hsu, I.C.; Wu, S.K.; Lin, R.Y. |
| 國立臺灣大學 |
1997 |
A Study on The Nickel-Riched Ternary Ti-Ni-Al Shape Memory Alloys
|
Hsieh, S.F.; 吳錫侃; Hsieh, S.F.; Wu, S.K. |
| 國立臺灣大學 |
1997 |
Ion Nitriding of Ti50Ni50 Shape Memory Alloy, Part I: Nitriding Parameters and Microstructure Characterization
|
吳錫侃; Lin, H.C.; Chu, C.L.; Wu, S.K.; Lin, H.C.; Chu, C.L. |
| 國立臺灣大學 |
1997 |
Ion Nitriding of Ti50Ni50 Shape Memory Alloy, Part II: Corrosion Properties
|
吳錫侃; Lin, H.C.; Chu, C.L.; Wu, S.K.; Lin, H.C.; Chu, C.L. |
| 國立臺灣大學 |
1997 |
Surface Modification of TiAl Intermetallics by Liquid Aluminizing
|
Hsu, I.C.; 吳錫侃; Lin, R.Y.; Hsu, I.C.; Wu, S.K.; Lin, R.Y. |
| 國立臺灣大學 |
1996 |
Oxidation Behavior of Equiatomic TiNi alloy in High Temperature Air Environment
|
Chu, C.L.; Wu, S.K.; Yen, Y.C. |
| 國立臺灣大學 |
1996 |
Ion nitriding of titanium aluminides with 25-53 at.% Al I: Nitriding parameters and microstructure characterization
|
Chu, C.L.; Wu, S.K. |
| 國立臺灣大學 |
1996 |
Liquid State Infrared Processing of SCS-6/Ti-6Al-4V Composites
|
Warrier, S.G.; Lin, R.Y.; Wu, S.K. |
| 國立臺灣大學 |
1996 |
Ion nitriding of titanium aluminides with 25-53 at.% Al II: Corrosion properties
|
Chu, C.L.; Wu, S.K. |
| 國立臺灣大學 |
1996 |
A Study on the Wire Drawing of TiNi Shape Memory Alloys
|
Wu, S.K.; Lin, H.C.; Yen, Y.C. |
| 國立臺灣大學 |
1996 |
Interface Characterization of Ceramic Fiber-Reinforced Ti Alloy Composites Manufactured by Infrared Processing
|
Warrier, S.G.; Chen, S.H.; Wu, S.K.; Lin, R.Y. |
| 臺大學術典藏 |
1996 |
A Study on the Wire Drawing of TiNi Shape Memory Alloys
|
WuSK; Yen, Y.C.; Lin, H.C.; Wu, S.K.; Wu, S.K.; Lin, H.C.; Yen, Y.C. |
| 國立臺灣大學 |
1995 |
Transformation Heat As a Function of Ternary Palladium Additions in Ti50Ni50-xPdx Alloys With X: 1-15 at.%
|
Lo, Y.C.; Wu, S.K. |
| 國立臺灣大學 |
1995 |
Shape Memory Intermetallics Development in Taiwan
|
Wu, S. K.; Lin, H. C. |
| 國立臺灣大學 |
1995 |
Analytical Electron Microscopy Study of A New Phase in an Equiatomic Ti50Pd50 Alloy
|
Chang, L.; Lo, Y.C.; Wu, S.K. |
| 國立臺灣大學 |
1995 |
A study on the dry uni-directional sliding behaviour of titanium aluminides
|
Chu, C.L.; Wu, S.K. |
| 國立臺灣大學 |
1995 |
Damping Characteristics of Ti50Ni49.5Fe0.5 and Ti50Ni40Cu10 Ternary Shape Memory Alloys
|
Lin, H.C.; Wu, S.K.; Chang, Y.C. |
| 國立臺灣大學 |
1995 |
A Study on Wear Characteristics of Titanium Aluminides With 25at% - 53at%Al
|
Chu, C.L.; 吳錫侃; Chu, C.L.; Wu, S.K. |
| 國立臺灣大學 |
1994 |
Effects of Cold Rolling on A Ti50Ni20Pd30 Alloy
|
Lo, Y.C.; Wu, S. K. |
| 國立臺灣大學 |
1994 |
The Tensile Behavior of A Cold-Rolled and Reverse-Transformed Equiatomic TiNi Alloy
|
Lin, H. C.; Wu, S. K. |
| 國立臺灣大學 |
1993 |
Damping Characteristics of TiNi Shape Memory Alloys
|
Lin, H.C.; Wu, S.K.; Yeh, M.T. |
| 國立臺灣大學 |
1993 |
A Study of High Resolution Electron Microscopy (HREM) on a α2+γTwo-Phase Ti-40 at% Al Alloy
|
Yang, Y.S.; Wu, S.K.; Wang, J.Y. |
| 國立臺灣大學 |
1993 |
Martensitic Transformation Sequence in a Ti50Ni47Pd3 Alloy
|
Lo, Y.C.; Wu, S.K. |
| 國立臺灣大學 |
1993 |
Determination of Heat of Transformation in a Cold-Rolled Martensitic TiNi Alloy
|
Lin, H.C.; Wu, S.K.; 林新智; 吳錫侃 |
| 臺大學術典藏 |
1992 |
Compositional dependence of martensitic transformation sequence in Ti50Ni50-xPdx alloys with X≤15at%
|
SHYI-KAAN WU;Wu, S.K.;Lo, Y.C.;SHYI-KAAN WU; Lo, Y.C.; Wu, S.K.; SHYI-KAAN WU |
| 國立高雄第一科技大學 |
1991.01 |
Orientation faults of γ lamellae in a Ti-40 at% Al alloy
|
Yang, Y.S;Wu, S.K; 楊玉森 |
| 國立臺灣大學 |
1991 |
The Tensile Properties of a Textured Ti65Al25Nb10 Alloy
|
Hon, W.P.; Wu, S.K.; Koo, C.H. |
| 國立臺灣大學 |
1991 |
The Effect of Precipitation Hardening on the Ms Temperature in a Ti49.2Ni50.8 Alloy
|
Wu, S.K.; Lin, H.C. |
| 國立臺灣大學 |
1991 |
Hot Processing and Toughness Improve-ment of The Ti3Al-Nb Alloy
|
Hon, W.P.; Koo, C.H.; Wu, S.K. |
| 國立臺灣大學 |
1991 |
A Study on The Basal Texture of a Ti65Al25Nb10 Alloy
|
Hon, W.P.; Koo, C.H.; Wu, S.K.; Chou, T.S. |
| 臺大學術典藏 |
1991 |
Heat of premartensitic transformation in an aged Ti49Ni51 alloy
|
Wu, S.K.; SHYI-KAAN WU; Lin, H.C. |
| 國立臺灣大學 |
1990 |
The Effect of Thermal Aging on a Ti50Ni10Au40 Alloy
|
Wu, S.K.; Lo, Y.C. |
| 國立臺灣大學 |
1990 |
Transformation Heat As a Function of Ternary Pd Additions in Ti50Ni50-xPdx Alloys With X:20-50 at.%
|
Lo, Y.C.; Wu, S.K.; Wayman, C.M. |
| 國立臺灣大學 |
1989 |
Transformation Temperatures of Martensite and Premartensite in an Aged Ti49Ni51 Alloy
|
Wu, S.K.; Lin, H.C.; Chou, T.S. |
| 國立臺灣大學 |
1987 |
System Design of Oxygen Probe and Microcomputer-Controlled Valve for Carbonitriding of Controlled Atmosphere
|
Wu, S.K.; Hsieh, S.F.; Hwang, C.H. |
| 國立臺灣大學 |
1985 |
The Carbon Potential of C-O, C-H, Mixture Gases on Steels in Vacuum at High Temperature
|
Wu, S.K.; Huang, T.Y.; Hwang, C.H. |
| 國立臺灣大學 |
1984 |
System Design of Oxygen Probe and Microcomputer-Controlled Valve for Carbon Potential of Controlled Atmosphere
|
Wu, S.K.; Hwang, C.H.; Lin, H.H. |